A Review of Corrosion and Hydrogen Diffusion Behaviors of High Strength Pipe Steel in Sour Environment
Sung Jin Kim, Kyoo Young Kim
J Weld Join. 2014;32(5):443-450. Published online 2014 Oct 30 DOI: https://doi.org/10.5781/JWJ.2014.32.5.13
|
Citations to this article as recorded by
Hydrogen embrittlement and hydrogen-induced crack initiation in additively manufactured metals: A critical review on mechanical and cyclic loading
Alireza Behvar, Meysam Haghshenas, Milos B. Djukic
International Journal of Hydrogen Energy.2024; 58: 1214. CrossRef Effect of wet Hydrogen Sulfide on Carbon Steels Degradation in Refinery Based on Case Study
Juliusz Orlikowski, Agata Jazdzewska, Ilyas Uygur, Radoslaw Gospos, Tomasz Olczak, Kazimierz Darowicki
Arabian Journal for Science and Engineering.2023; 48(7): 9171. CrossRef Studying the temperature influence on carbon steel in sour petroleum media using facilely-designed Schiff base polymers as corrosion inhibitors
Olfat E. El-Azabawy, Shimaa A. Higazy, Ahmed M. Al-Sabagh, Adel A.H. Abdel-Rahman, Notaila M. Nasser, Eman A. Khamis
Journal of Molecular Structure.2023; 1275: 134518. CrossRef Hydrogen-induced cracking and blistering in steels: A review
May L. Martin, Petros Sofronis
Journal of Natural Gas Science and Engineering.2022; 101: 104547. CrossRef Study of Electrochemical Behavior, Hydrogen Permeation and Diffusion in Pipeline Steel
Swapna Dey, Seetharaman Sivaprasad, Nityananda Das, Indranil Chattoraj
Materials Science Forum.2021; 1019: 145. CrossRef Hydrogen-Induced Cracking Caused by Galvanic Corrosion of Steel Weld in a Sour Environment
Jin Sung Park, Jin Woo Lee, Sung Jin Kim
Materials.2021; 14(18): 5282. CrossRef A Comparative Investigation of the Corrosion Resistance and HIC Suceptibility of API 5L X65 and API 5L X80 Steels
Janeth Marlene Quispe-Avilés, Duberney Hincapie-Ladino, Neusa Alonso Falleiros, Hercílio Gomes de Melo
Materials Research.2019;[Epub] CrossRef Hydrogen diffusion in low alloy steels under cyclic loading
Marina Cabrini, Sergio Lorenzi, Tommaso Pastore, Diego Pesenti Bucella
Corrosion Reviews.2019; 37(5): 459. CrossRef Effect of thermomechanical processing on hydrogen permeation in API X70 pipeline steel
Hossein Izadi, Masoomeh Tavakoli, Mohammad Hadi Moayed
Materials Chemistry and Physics.2018; 220: 360. CrossRef Corrosion problems in the oil country tubular goods and their mitigation – a review
Shan Cao, Faqing He, Jinwei Gao
Anti-Corrosion Methods and Materials.2017; 64(5): 465. CrossRef Influence of hydrogen on mechanical properties and fracture of tempered 13 wt% Cr martensitic stainless steel
B. Sunil Kumar, Vivekanand Kain, Manpreet Singh, B. Vishwanadh
Materials Science and Engineering: A.2017; 700: 140. CrossRef Numerical study on hydrogen permeation of ferritic steel evaluated under constant load
S. J. Kim, D. W. Yun, H. G. Jung, K. Y. Kim
Materials Science and Technology.2017; 33(2): 149. CrossRef Critical Assessment 17: Mechanisms of hydrogen induced cracking in pipeline steels
K. O. Findley, M. K. O'Brien, H. Nako
Materials Science and Technology.2015; 31(14): 1673. CrossRef
|