The Effect of Interpass Peening on Mechanical Properties in Additive Manufacturing of Ti-6Al-4V
Jae-Gyu Byun, Hui-jun Yi, Sang-Myung Cho
J Weld Join. 2017;35(2):6-12.   Published online 2017 Apr 28     DOI: https://doi.org/10.5781/JWJ.2017.35.2.2
Citations to this article as recorded by Crossref logo
Effect of Machine Hammer Peening Conditions on β Grain Refinement of Additively Manufactured Ti-6Al-4V
Leonor Neto, Stewart Williams, Alec E. Davis, Jacob R. Kennedy
Metals.2023; 13(11): 1888.     CrossRef
The Effect of Decomposed Microstructure on Mechanical Properties of Additively Manufactured Ti-6Al-4V Alloy
Desrilia Nursyifaulkhair, Nokeun Park, Eung Ryul Baek
Journal of Welding and Joining.2021; 39(5): 527.     CrossRef
The Effectiveness of Grain Refinement by Machine Hammer Peening in High Deposition Rate Wire-Arc AM Ti-6Al-4V
J. R. Hönnige, A. E. Davis, A. Ho, J. R. Kennedy, L. Neto, P. Prangnell, S. Williams
Metallurgical and Materials Transactions A.2020; 51(7): 3692.     CrossRef
Microstructure and mechanical properties of CoCrFeMnNi high entropy alloy with ultrasonic nanocrystal surface modification process
Timothy Alexander Listyawan, Hyunjong Lee, Nokeun Park, Unhae Lee
Journal of Materials Science & Technology.2020; 57: 123.     CrossRef