Effect of Burn-off Length on the Properties of Friction Welded Dissimilar Steel Bars
Muralimohan Cheepu, Woo Seong Che
J Weld Join. 2019;37(1):46-55.   Published online 2019 Jan 18     DOI: https://doi.org/10.5781/JWJ.2019.37.1.6
Citations to this article as recorded by Crossref logo
Microstructure and Mechanical Properties of the Bimetallic Wire Arc Additively Manufactured Structure (BAMS) of SS304L and SS308L Fabricated by Hybrid Manufacturing Process
Sirisha Bhadrakali Ainapurapu, Venkata Anantha Ramasastry Devulapalli, Ram Prabhu Theagarajan, Bharat Kumar Chigilipalli, Ravi Kumar Kottala, Muralimohan Cheepu
Transactions of the Indian Institute of Metals.2023; 76(2): 419.     CrossRef
Analysis on Bonding Interface during Solid State Additive Manufacturing between 18Cr-8Ni and 42CrMo4 High Performance Alloys
Syed Quadir Moinuddin, Venkata Varalakshmi Machireddy, Vadla Raghavender, Tejonadha Babu Kaniganti, Venukumar Sarila, Shankar Madhuraveli Ponnappan, Ragavanantham Shanmugam, Muralimohan Cheepu
Metals.2023; 13(3): 488.     CrossRef
Microstructure and Mechanical Properties of Solid-State Rotary Friction Welded Inconel 713C and 32CrMo4 Steel Joints Used in a Turbocharger Rotor
Krzysztof Szwajka, Joanna Zielińska-Szwajka, Tomasz Trzepieciński
Materials.2023; 16(6): 2273.     CrossRef
Experimental investigations and effect of parameters on friction welded AISI 304 and Invar alloys
Jignesh Patel, Bimal Kumar Mawandiya, Kaushik Patel, Mayur A. Makhesana, Manish Gupta, Karrar Hazim Salem, Satbir S. Sehgal
Advances in Materials and Processing Technologies.2023; : 1.     CrossRef
Laser welding of dissimilar alloys between high tensile steel and Inconel alloy for high temperature applications
Muralimohan Cheepu, Y. Ashok Kumar Reddy, S. Indumathi, D. Venkateswarlu
Advances in Materials and Processing Technologies.2022; 8(2): 1197.     CrossRef
Effect of filler materials on dissimilar TIG welding of Inconel 718 to high strength steel
Anuradha M., Chittaranjan Das Vemulapalli, Muralimohan Cheepu
Materials Today: Proceedings.2022; 52: 1314.     CrossRef
Influence of joint interface on mechanical properties in dissimilar friction welds
Muralimohan Cheepu, Harinadh Cheepu, Karpagaraj A, Woo Seong Che
Advances in Materials and Processing Technologies.2022; 8(1): 732.     CrossRef
Effects of Heat Treatment on the Mechanical Behavior of Udimet 720 Nickel-Based Superalloy
Yu Sik Kong, Muralimohan Cheepu, Dong Gyu Kim
Journal of Materials Engineering and Performance.2022; 31(10): 8327.     CrossRef
Dissimilar metals TIG welding-brazing of AZ31 magnesium alloy to 304 stainless steel
Sairam Kotari, Eshwaraiah Punna, S.M. Gangadhar, Muralimohan Cheepu, P. Sarkar, S. Venukumar
Materials Today: Proceedings.2021; 39: 1549.     CrossRef
Evaluation of the mechanical properties of Inconel 718 to SCM 440 dissimilar friction welding through real-time monitoring of the acoustic emission system
Yu Sik Kong, Muralimohan Cheepu, Jin-Kyung Lee
Proceedings of the Institution of Mechanical Engin.2021; 235(5): 1181.     CrossRef
Dissimilar Rotary Friction Welding of Inconel 718 to F22 Using Inconel 625 Interlayer
Ateekh Ur Rehman, Nagumothu Kishore Babu, Mahesh Kumar Talari, Saqib Anwar, Yusuf Usmani, Ali M. Al-Samhan
Applied Sciences.2021; 11(22): 10684.     CrossRef
Influence of Friction Pressure on Microstructure and Joining Phenomena of Dissimilar Joints
Muralimohan Cheepu, Woo Seong Che
Transactions of the Indian Institute of Metals.2020; 73(6): 1455.     CrossRef
Interface Microstructure Characteristics of Friction-Welded Joint of Titanium to Stainless Steel with Interlayer
Muralimohan Cheepu, P. Susila
Transactions of the Indian Institute of Metals.2020; 73(6): 1497.     CrossRef
Growth Rate of Intermetallics in Aluminum to Copper Dissimilar Welding
Muralimohan Cheepu, P. Susila
Transactions of the Indian Institute of Metals.2020; 73(6): 1509.     CrossRef
Characterization of Interfacial Microstructure in Friction Welds Between Inconel 718 and SM45C Steel
Muralimohan Cheepu, Woo Seong Che
Transactions of the Indian Institute of Metals.2020; 73(6): 1567.     CrossRef
Influence of rotational speed on the dissimilar friction welding of heat-treated aluminum alloys
G. Ravi Chandra, S. Venukumar, Muralimohan Cheepu
IOP Conference Series: Materials Science and Engin.2020; 998(1): 012070.     CrossRef
Characterization of Microstructure and Interface Reactions in Friction Welded Bimetallic Joints of Titanium to 304 Stainless Steel Using Nickel Interlayer
Muralimohan Cheepu, Woo-Seong Che
Transactions of the Indian Institute of Metals.2019; 72(6): 1597.     CrossRef
Friction Welding of Titanium to Stainless Steel Using Al Interlayer
Muralimohan Cheepu, Woo Seong Che
Transactions of the Indian Institute of Metals.2019; 72(6): 1563.     CrossRef
The Role of Material Location on the First Mode of Metal Transfer and Weld Formation in Dissimilar Friction Stir Welded Thin Sheets
K. Tejonadha Babu, S. Muthukumaran, C. H. Bharat Kumar
Transactions of the Indian Institute of Metals.2019; 72(6): 1589.     CrossRef
Influence of Temperature on Impact Sensitivity of Matchhead Composition while in Contact with Different Process Materials
S.P. Sivapirakasham, K. Harisivasri Phanindra, Mahadevan Surianarayanan, K.R. Balasubramanian
Materials Science Forum.2019; 969: 55.     CrossRef
The Influence of Gas Tungsten Arc Welding Parameters on Mechanical and Microstructure Properties of the TC4 Titanium Alloy
Muralimohan Cheepu, D. Venkateswarlu, P. Nageswara Rao, S. Senthil Kumaran, Narayanan Srinivasan
Materials Science Forum.2019; 969: 895.     CrossRef
Influence of Different In-Process and Building Materials with Varying Hardness on Impact Sensitivity of the Matchhead Composition
S.P. Sivapirakasam, K. Harisivasri Phanindra, Mahadevan Surianarayanan, K.R. Balasubramanian
Materials Science Forum.2019; 969: 41.     CrossRef
Microstructure Characterization of Superalloy 718 during Dissimilar Rotary Friction Welding
Muralimohan Cheepu, D. Venkateswarlu, P. Nageswara Rao, V. Muthupandi, Katakam Sivaprasad, Woo Seong Che
Materials Science Forum.2019; 969: 211.     CrossRef
Cold Metal Transfer (CMT) Welding of Dissimilar Materials: An Overview
S. Venukumar, Muralimohan Cheepu, T. Vijaya Babu, D. Venkateswarlu
Materials Science Forum.2019; 969: 685.     CrossRef
Characterization of Microstructure and Mechanical Properties of AA2219-O and T6 Friction Stir Welds
D. Venkateswarlu, Muralimohan Cheepu, P. Nageswara Rao, S. Senthil Kumaran, Narayanan Srinivasan
Materials Science Forum.2019; 969: 205.     CrossRef
Effect of Process Parameters and Heat Input on Weld Bead Geometry of Laser Welded Titanium Ti-6Al-4V Alloy
Muralimohan Cheepu, D. Venkateswarlu, P. Nageswara Rao, S. Senthil Kumaran, Narayanan Srinivasan
Materials Science Forum.2019; 969: 613.     CrossRef