A Study on Servo DC Resistance Spot Welding of Mg Alloy Sheet(1)
SunNyeo Jung, HeeSeok Chang, Mok-Young Lee


Correspondence:   Published online March 12, 2009
ABSTRACT
  Weldability of Mg alloy was investigated using servo-actuated DC resistance spot welder. Due to its uncommon electrical and mechanical properties, lots of voids and cracks were observed inside nugget with conventional weld schedule. Lobe curve was proposed to clarify proper electrode force and weld current, which guarantee reasonable weld strength and fatigue life. Macro structure of sectioned specimen was examined to count total number of void and crack. Post weld schedule is also proposed to reduce micro vickers hardness value of weld zone.
Keywords: Mg alloy;Servo-actuated resistance Spot welder;Lobe curve;Dynamic resistance
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,219
View
0
Download
Related articles
The Effect of Pre-Welding on Nugget Growth Behavior and Weldability for the Resistance Spot Welding of A6014 - T4 Alloy  2020 April;38(2)
Effects of Electrode Face Thickness on Resistance Spot Weldability of Aluminium Alloy 6061  2020 February;38(1)
A Study for the Characteristics of Laser Welding on Over-lap Joint of Thin Magnesium Alloy Sheet  2019 August;37(4)
Effects of Electrode Face Radius and Force on Resistance Spot Weldability of Aluminium Alloy 6061  2018 December;36(6)
A Comparative Study of Weldable Current Range on AC and MFDC Resistance Spot Welding for 440 MPa Grade Steel Sheet   2017 February;35(1)
The Effect of Pre-Welding on Nugget Growth Behavior and Weldability for the Resistance Spot Welding of A6014 - T4 Alloy  2020 April;38(2)
Effects of Electrode Face Thickness on Resistance Spot Weldability of Aluminium Alloy 6061  2020 February;38(1)
A Study for the Characteristics of Laser Welding on Over-lap Joint of Thin Magnesium Alloy Sheet  2019 August;37(4)
Effects of Electrode Face Radius and Force on Resistance Spot Weldability of Aluminium Alloy 6061  2018 December;36(6)
A Comparative Study of Weldable Current Range on AC and MFDC Resistance Spot Welding for 440 MPa Grade Steel Sheet   2017 February;35(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.