Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Process Parameter Effect on Deformation of a V-groove Thin Plate for FCAW and EGW

J Weld Join > Volume 31(1); 2013 > Article
Journal of KWJS 2013;31(1):65-70.
DOI: https://doi.org/10.5781/KWJS.2013.31.1.65    Published online June 5, 2013.
Process Parameter Effect on Deformation of a V-groove Thin Plate for FCAW and EGW
Juho Han, Jaeseung Jeon, Chulsung Park, Chongin Oh, Jinoh Yun, Jeongsoo Lee
Correspondence:  Jeongsoo Lee,
Email: leejszz@hanjinsc.com
Abstract
Finite element analysis and welding experiments were performed to evaluate deformation aspect for Flux Cored Arc Welding(FCAW) and Electro Gas Welding(EGW). Numerical researches of FCAW and EGW were performed considering the difference of number of welding pass and welding direction to arc flow. To perform the numerical study of FCAW and EGW, number of welding pass and welding direction to arc flow were considered in the finite element model. FCAW process requires multi pass and its welding direction is vertical to welding torch. On the other hand, EGW process requires single pass and its welding direction is parallel to welding torch. The difference of welding direction and heat input was considered in the finite element analysis. In FCAW process, Goldak’s double ellipsoidal heat input model was adopted. In the EGW process, Hemi-spherical power density distribution was adopted. In the results of experiment and finite element analysis, angular deformation of FCAW process is larger than that of EGW process.
Key Words: FCAW, EGW, Deformation, Finite element analysis, Goldak
TOOLS
METRICS Graph View
  • 0 Crossref
  •    
  • 5,375 View
  • 0 Download
Related articles


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI