6
-
Journal of KWJS. 2013;31(1):11-20. Published online June 4, 2013.
DOI: https://doi.org/10.5781/KWJS.2013.31.1.11
- Recent Study of Overlay Welding on Welding methods
-
Ho-Cheon Yoo
-
- Corresponding author: Ho-Cheon Yoo ,Email: yooho278@reseat.re.kr
- Abstract
- Recent developing tendency of overlay welding on welding methods are studied by searching of NDSL, ScienceDirect and KIPRIS. PTA, Laser cladding, SMAW, GTAW, GMAW, SAW and ESW are selected as welding methods. Development and improvement of various new overlay welding processes and technology are introduced, especially PTA and Laser cladding in abroad overlay welding technology are activated substantially.
Keywords :Overlay welding, PTA, Laser cladding, SMAW, GTAW, GMAW, SAW. ESW