Review Paper

  • HOME
  • ARTICLE CATEGORY
  • Review Paper
A Review on Twin Tungsten Inert Gas Welding Process Accompanied by Hot Wire Pulsed Power Source
Prassan Shah, Chetan Agrawal
J Weld Join. 2019;37(2):41-51.   Published online April 8, 2019
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032015
Epoxy Polymer Solder Pastes for Micro-Electronic Packaging Applications
Ashutosh Sharma, Do Hyun Jung, Ju Seon Cheon, Jae Pil Jung
J Weld Join. 2019;37(2):7-14.   Published online April 30, 2019
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031978
Recent Joining Techniques of CFRP to Metal Using Welding Process
Yong Kim, Hee-seon Bang
J Weld Join. 2018;36(5):27-38.   Published online October 22, 2018
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031981
Laser and Gas Metal Arc Based Dissimilar Joining of Automotive Aluminium Alloys and Steel Sheets - A Review
Atanu Das, Hee-Seon Bang
J Weld Join. 2018;36(5):1-11.   Published online October 26, 2018
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
A Review on Welding Residual Stress Measurement by Hole Drilling Technique and its Importance
R. Chakrabarti, P. Biswas, S. C. Saha
J Weld Join. 2018;36(4):75-82.   Published online July 23, 2018
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Review of Keyhole Refilling Technology in Friction Stir Welding
Jin Young Yoon, Sanghoon Kang, Sehun Rhee, Cheolhee Kim
J Weld Join. 2018;36(4):58-62.   Published online July 20, 2018
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031716
The Current State, Outcome and Vision of Additive Manufacturing
Mathieu Terner
J Weld Join. 2015;33(6):1-5.   Published online December 31, 2015
PDFPDF    
2031706
Influence of Various Additional Elements in Al Based Filler Alloys for Automotive and Brazing Industry
Ashutosh Sharma, Y.S. Shin, Jae-Pil Jung
J Weld Join. 2015;33(5):1-8.   Published online October 30, 2015
PDFPDF    
Mechanical fastening and joining technologies to using multi mixed materials of car body
Yong Kim, Ki-Young Park, Sung-Bok Kwak
J Weld Join. 2015;33(3):12-18.   Published online June 30, 2015
PDFPDF    
2031685
High efficient welding technology of the offshore wind power plants
Youngsik Kim, Sangcheol Kil
J Weld Join. 2015;33(3):4-11.   Published online June 30, 2015
PDFPDF    
Recent study of materials and welding methods for nuclear power plant
Ho-Cheon Yoo
J Weld Join. 2015;33(1):14-23.   Published online February 28, 2015
PDFPDF    
2031659
Review of magnetic pulse welding
Bong-Yong Kang
J Weld Join. 2015;33(1):7-13.   Published online February 28, 2015
PDFPDF    
2031602
Numerical Studies on Submerged Arc Welding Process
Degala Ventaka Kiran, Suck-Joo Na
J Weld Join. 2014;32(4):339-347.   Published online August 30, 2014
PDFPDF    
2031587
Experimental Studies on Submerged Arc Welding Process
Degala Ventaka Kiran, Suck-Joo Na
J Weld Join. 2014;32(3):215-224.   Published online June 30, 2014
PDFPDF    
Recent Study in Variation of Welding Materials for Overlay Welding
Ho-Cheon Yoo
J Weld Join. 2013;31(6):17-26.   Published online January 21, 2014
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.

ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI