577 Recrystallization Behavior of CP Ti Welds by Rolling   
Byoung-Hyun Yoon, Ji-Yeon Shim, Bong-Yong Kang
Journal of Welding and Joining:577-581.  Publication Date (Web): December 9, 2021
                  PDF Links
 
582 Effect of Post-Weld Heat Treatment Temperature on the Mechanical Properties and Microstructure of Carbon Steel Base Metal   
Yongjoon Kang, Chang-Young Oh, Seung-Gun Lee, Sanghoon Lee, Sung-Sik Kang
Journal of Welding and Joining:582-589.  Publication Date (Web): December 27, 2021
                  PDF Links
 
590 Optimization of Additive Manufacturing of Precipitation Hardening Type STS630 by DED (Direct Energy Deposition) Process   
Yongjae Kwon, SeongSeon Shin, SangEun Joo, JongHoon Lee, JunHo Hwang, HyunDeok Kim
Journal of Welding and Joining:590-596.  Publication Date (Web): December 27, 2021
                  PDF Links
 
597 Electromagnetic Self-Piercing Riveting (E-SPR) Process for Dissimilar Materials Joints   
Seon-Ho Nam, Bong-Yong Kang, Min-Woo Park, Sung-Jin Park, Ji-Yeon Shim
Journal of Welding and Joining:597-602.  Publication Date (Web): December 27, 2021
                  PDF Links
 
603 Review on the Wire Arc Additive Manufacturing Process and Trends in Non-ferrous Alloys   
Jae-Deuk Kim, Joo Yong Cheon, Changwook Ji
Journal of Welding and Joining:603-612.  Publication Date (Web): December 6, 2021
                  PDF Links
 
613 Dimension Precision and Uniformability Depending on the Interpass Distance Variation of Automated-Wire Arc Additive Manufacturing using 5 Cr-4 Mo Tool Steel Alloy   
Jae-Deuk Kim, Jae Won Kim, Joo Yong Cheon, Sungwook Kang, Yeong-Do Park, Changwook Ji
Journal of Welding and Joining:613-624.  Publication Date (Web): December 6, 2021
                  PDF Links
 
625 Property Evaluation and Fabrication of WC-Co-Si3N4 Hard Materials by a Rapid Sintering Process   
Jeong-Han Lee, Hyun-Kuk Park
Journal of Welding and Joining:625-631.  Publication Date (Web): December 6, 2021
                  PDF Links
 
632 Study on the Improvement of TIG Welding Productivity through Analysis of ArcTig Welding Properties   
Sung-Hyun Jeon, Tae-Wan Kim, Young-Woong Lee, Yu-Chan Kim
Journal of Welding and Joining:632-640.  Publication Date (Web): December 6, 2021
                  PDF Links
 
641 Study on the Microstructure and Mechanical Properties of Butt GMAW Al/Fe Dissimilar Joints using Pure Copper Filler Metal   
Ju-Hee Jung, Dae-Woong Park, Eung-Ryul Baek
Journal of Welding and Joining:641-648.  Publication Date (Web): December 9, 2021
                  PDF Links
 
649 Study on Nugget Diameter Prediction of Resistance Spot Welding Using an Artificial Neural Network   
Jongkyu Kim, JaHun Ku, Yeongdo Park, Youngchang Kim, Youngmin Hwang, Heesoo Kim, Sivaprasad Murugan, Namkug Ku
Journal of Welding and Joining:649-657.  Publication Date (Web): December 6, 2021
                  PDF Links
 
658 Machine Learning Modeling and Hyper-Parameter Optimization for Weld Nugget Formation and Failure Behavior of Resistance Spot Welds   
Hyeonjeong You, Cheolhee Kim
Journal of Welding and Joining:658-665.  Publication Date (Web): December 8, 2021
                  PDF Links
 
666 Process Review on Dissimilar Metal Joining of Steel and Ti Alloys   
Hyeonjeong You, Taehyun Lee, Minjung Kang, Cheolhee Kim
Journal of Welding and Joining:666-676.  Publication Date (Web): December 6, 2021
                  PDF Links
 
677 Microstructural Evolution of Cantilever Wire Probe after Touch-Down Fatigue Cycles for Power Semi-Conductor Wafer Testing   
Won Sik Hong, Mi-Song Kim, Myeongin Kim
Journal of Welding and Joining:677-683.  Publication Date (Web): December 6, 2021
                  PDF Links
 
684 Hot Ductility Behavior in the Weld Heat-Affected Zone of Austenitic Fe-Mn-Al-C Lightweight Steels and the Effects of Alloying Elements   
Joonoh Moon
Journal of Welding and Joining:684-689.  Publication Date (Web): December 27, 2021
                  PDF Links
 
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI