Search

  • HOME
  • Search
2032221
A Review of the Brazeability of Low-Temperature and Nano-Reinforced Al-Based Brazing Filler Metals
Furkan, Hye-Jeong Kim, Gun-hwan Lee, Jae Pil Jung
J Weld Join. 2022;40(3):216-224.   Published online June 17, 2022
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Formation of Intermetallic Compounds at the Interface of the Friction Stir Weld and Diffusion Bond of Mg-AZ31/Al-5083 Joint
Mohammad Ammar Mofid, Ehsan Loryaei, Mostafa Hajian Heidary
J Weld Join. 2019;37(6):591-598.   Published online December 5, 2019
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Laser Cladding by Printing Si Powder Paste on A1050 Al Alloy Surface
Hyoung-Keun Lee
J Weld Join. 2018;36(1):57-64.   Published online January 26, 2018
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Microstructure Evolution and Corrosion Behavior in the Welds of High Interstitial FeCrMnNC Austenitic Stainless Steels
Joonoh Moon, Heon-Young Ha, Tae-Ho Lee
J Weld Join. 2017;35(4):51-57.   Published online July 21, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Laser Cladding with Al-36%Si Powder Paste on A319 Al Alloy Surface to Improve Wear Resistance
Hyoung-Keun Lee
J Weld Join. 2017;35(2):58-62.   Published online April 28, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031706
Influence of Various Additional Elements in Al Based Filler Alloys for Automotive and Brazing Industry
Ashutosh Sharma, Y.S. Shin, Jae-Pil Jung
J Weld Join. 2015;33(5):1-8.   Published online October 30, 2015
PDFPDF    
Process Evaluation of Plasma-GMA Welding for Al 5052 and 6061 Alloy
Cheolhee Kim, Young-Nam Ahn, Jin-Kang Choi, Sehun Rhee
J Weld Join. 2010;28(6):58-62.   Published online January 10, 2011
PDFPDF    
The Development of Welding Process to Prevent Porosity in MIG Welding of Al 6082-T6
Sang-Yeub Baek, Yon-Ho Jung, Won-Il Kim, Sang-Myung Cho
J Weld Join. 2010;28(6):28-34.   Published online January 10, 2011
PDFPDF    
Microstructure and Mechanical Properties of Clad(A4045/A3003) Al Alloy by Gas Tungsten Arc Welding
Ki-Bin Kim, Jin-Seon Gook, Dong-Ju Yoon, Byung-Il Kim, Il-Cheon Lee
J Weld Join. 2008;26(4):73-78.   Published online September 24, 2008
PDFPDF    
Microstructure and Mechanical Properties of A3003 Aluminium Alloy Welds by Heat-treatment
Il-Cheon Lee, Yeong-Jong Song, Jin-Seon Gook, Dong-Joo Yoon, Byung-Il Kim
J Weld Join. 2007;25(5):51-57.   Published online December 3, 2007
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI