74 A Study on the Defect Detection Algorithm by Interval Statistical Processing Method of Arc Welding Waveform   
Woo-Hyeon Ju, Hyeong-Chang Ryu, Kyeong-Seob Lim, Jong-Jung Lee, Yong-Hwan Park, Sang-Myung Cho
Journal of Welding and Joining:74-80.  Publication Date (Web): February 3, 2021
                  PDF Links
 
480 Defect Detection in Friction Stir Welding by Online Infrared Thermography   
Igor Kryukov, Michael Hartmann, Stefan Böhm, Malte Mund, Klaus Dilger, Fabian Fischer
Journal of Welding and Joining:480-487.  Publication Date (Web): October 30, 2014
PDF Links
 
1 |
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI