Quality Prediction Algorithm for Flow Drilling Screw Joining of 590 MPa High-Strength Steel and 6xxx Series Aluminum Alloy
Yu Ri Choi, Dong Yoon Kim, Jun Myoung ang, Ji Young Yu, Seung Hwan Lee
J Weld Join. 2024;42(4):366-377.   Published online August 31, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032314
A Study on the Residual Stress of Seam Pipe Cutting and Girth Welding
Ji-Sun Roh, Myung-Su Yi, Jung-Goo Park, Myung-Hyun Kim
J Weld Join. 2024;42(1):27-40.   Published online February 28, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032025
Experimental Investigation of Infrared Laser Drilling Process Applied with Different Repetition Rate on Ni-Au Coated BeCu
Seungik Son, Dongkyoung Lee
J Weld Join. 2019;37(3):206-211.   Published online June 27, 2019
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032023
Process Optimization for Femtosecond Laser Hole Drilling of Silicon Wafer
Hyeongwon Kim, Hyungson Ki
J Weld Join. 2019;37(3):220-225.   Published online June 26, 2019
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032022
CO2 Laser Drilling Processing of the Cover Glass using the Taguchi Method
Joonghan Shin, Donghyeok Choi
J Weld Join. 2019;37(3):199-205.   Published online June 17, 2019
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
A Review on Welding Residual Stress Measurement by Hole Drilling Technique and its Importance
R. Chakrabarti, P. Biswas, S. C. Saha
J Weld Join. 2018;36(4):75-82.   Published online July 23, 2018
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2026 by The Korean Welding and Joining Society.

Developed in M2PI