Solder Joint Degradation and Electrochemical Metallic Ion Migration Property of Solder Joints with Surface Finish
Hye Min Lee, Mi-Song Kim, Won Sik Hong
J Weld Join. 2023;41(4):265-274.   Published online August 31, 2023
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032222
Effects of Solder Powder Particle Size and Substrate Surface Finish on Degradation Properties of Solder Joints
Mi-Song Kim, Won Sik Hong, Hye-Min Lee, Myeongin Kim
J Weld Join. 2022;40(3):207-214.   Published online June 20, 2022
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Review on Vacuum Laser Beam Welding
Yongki Lee, Jason Cheon, Cheolhee Kim
J Weld Join. 2022;40(1):74-83.   Published online February 9, 2022
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031687
A study of joint properties of Sn-Cu-(X)Al(Si) middle-temperature solder for automotive electronics modules
Dong-Yurl Yu, Yong-Ho Ko, Junghwan Bang, Chang-Woo Lee
J Weld Join. 2015;33(3):19-24.   Published online June 30, 2015
PDFPDF    
Correlation of Microstructure and Tribological Properties of Mo Blended Fe-Base Coatings Fabricated by Atmospheric Plasma Spraying
Illjoo Lee, Hyungkwon Park, Changhee Lee
J Weld Join. 2014;32(5):495-501.   Published online October 30, 2014
PDFPDF    
Microstructure Evolution of Cu-based BMG Coating during APS Process and Phase Analysis by Nano-indentation Test
Junghwan Kim, Kicheol Kang, Sanghoon Yoon, Hyuntaek Na, Changhee Lee
J Weld Join. 2009;27(6):43-48.   Published online January 13, 2010
PDFPDF    
Characterization of Ni/YSZ Anode Coating for Solid Oxide Fuel Cells by Atmospheric Plasma Spray Method
Soodong Park, Sanghoon Yoon, Kicheol Kang, Changhee Lee
J Weld Join. 2008;26(4):50-54.   Published online September 24, 2008
PDFPDF    
Characteristics of Plasma Sprayed TiO₂-NiCr Conductive Heating Roll Coatings
Tae-Gu Kang, Min-Seok Jin, Young-Bong Ko et al.
J Weld Join. 2007;25(4):28-34.   Published online September 21, 2007
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI