Laser Cutting Characteristics Using High-speed Camera of 75-㎛ Thick Stainless Steel Foil in Lightweight Fuel Cell Applications
Jung-Lo Yoon, Su-Jin Lee, Ryoon-Han Kim, Kwang-Deok Choi, NamHyun Kang, Danbi Song
J Weld Join. 2024;42(6):635-646.   Published online December 31, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032357
Characteristics of Solidification Cracking for Ni-P Coated Cu-Al5052 Single-Mode Fiber Laser Welds
Ye-Ji Yoo, Eun-Joon Chun
J Weld Join. 2024;42(5):472-480.   Published online October 31, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032292
Hot Cracking Characteristics During Single-Mode Fiber and Green Laser Welding Processes in Lithium-Ion Battery Pack Manufacturing (Editors’ Choice)
Jae-Hyeon Park, Myung-Jin Kim, Heeshin Kang, Wonah Park, Eun-Joon Chun
J Weld Join. 2023;41(5):367-378.   Published online October 31, 2023
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032280
Solidification Crack Free Welding Strategy via Ultra High Precision Laser Scanning at a Single Grain of Directionally Solidified and Single Crystal Superalloys
Seong-Jin Lee, Kyeong-Min Kim, Heeshin Kang, Seong-Moon Seo, Wonah Park, Eun-Joon Chun
J Weld Join. 2023;41(4):254-264.   Published online August 31, 2023
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Mechanical Properties of Cu and Ni Dissimilar Welds by High Welding Speed Using Single-Mode Fiber Laser
Su-Jin Lee, Jong-Do Kim
J Weld Join. 2014;32(3):295-302.   Published online June 30, 2014
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2026 by The Korean Welding and Joining Society.

Developed in M2PI