A Force Based Determination of Hot Cracking Susceptibility
Philipp Liepold, Arne Kromm, Thomas Kannengiesser
J Weld Join. 2025;43(4):447-457.   Published online August 31, 2025
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032397
Analysis of Resistance Spot Welding Characteristics with Flat Electrodes for Reducing Indentation in Excavator Exterior Parts
Young-Min Kim, Seung Hwan Lee, Insung Hwang
J Weld Join. 2025;43(2):176-184.   Published online April 30, 2025
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032361
Quality Classification of Multi-Layer Copper Foil Stacks Welds for Ultrasonic Welding Using CNN and RNN
Seon-myoung Hong, Jae-woo Cho, Hee-seon Bang
J Weld Join. 2024;42(5):514-520.   Published online October 31, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Trend of Resistance Spot Welding Technology of Al-Si Coated Hot-Stamped Boron Steel for Automobile Body
Wonho Kim, Changwook Ji
J Weld Join. 2022;40(2):187-197.   Published online April 15, 2022
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Recent Trends to Improve Laser Weldability of Al-Si coated Hot-stamped Boron Steel
Hyunuk Jun, Changwook Ji
J Weld Join. 2022;40(2):175-186.   Published online April 15, 2022
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032066
Effect of the Melting Behavior of the Coating Layer on Weldability in the Bolt Projection Resistance Welding of Al-Si Coated Hot-Stamped Boron Steel
Jae-Hun Kim, Hyun-Uk Jun, Joo-Yong Cheon, Yang-Do Kim, Changwook Ji
J Weld Join. 2020;38(1):33-40.   Published online February 19, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032036
A Study for the Characteristics of Laser Welding on Over-lap Joint of Thin Magnesium Alloy Sheet
Mokyoung Lee, Jaej Kim
J Weld Join. 2019;37(4):293-298.   Published online August 29, 2019
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031917
The Resistance Spot Weldability of a Stainless Steel/Aluminium/Low Carbon Steel 3-Ply Clad Sheet
Siva Prasad Murugan, Muralimohan Cheepu, Vijeesh Vijayan, Changwook Ji, Yeong-Do Park
J Weld Join. 2018;36(1):25-33.   Published online February 14, 2018
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031862
The Effects of PWHT on Tensile Properties and Microstructures for Laser Welds of Ti-6Al-4V Alloys
Yool Byun, Sangwon Lee, Chanhee Park, Jongtaek Yeom, Namhyun Kang, JaeKeun Hong
J Weld Join. 2017;35(4):1-5.   Published online August 14, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031752
Short Circuit Waveform Control Type SMAW Welding Power Source Development and Characteristic Evaluation
Hyun-Min Yang, Hoi-Soo Ryoo, Soong-Keun Hyun
J Weld Join. 2016;34(3):40-46.   Published online June 30, 2016
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031586
Resistance Spot Welding Characteristics of Mg Alloy Applying Current Waveform Control
Dong-Soon Choi, In-Sung Hwang, Dong-Cheol Kim, Jae-Wook Ryu, Moon-Jin Kang
J Weld Join. 2014;32(2):196-201.   Published online May 14, 2014
PDFPDF    
2031574
Weldability Increase of Aluminum by Variable Polarity Arc
Jungho Cho
J Weld Join. 2014;32(1):108-111.   Published online February 27, 2014
PDFPDF    
2031551
Effects of High Current and Welding Wire Diameter on the Magnesium Vaporization and Mechanical Properties of Al5083 Arc Welds
Heimi Kwon , Chul-ho Park , In-Pyo Hong , Namhyun Kang
J Weld Join. 2013;31(6):84-89.   Published online January 21, 2014
PDFPDF    
A Study for Resistance Spot Weldability of Pre-sealed Sheet Steel for Automobile Body by Using Pre-current
Taegyu Park, Sangman Yun, Sehun Rhee
J Weld Join. 2009;27(6):36-42.   Published online January 13, 2010
PDFPDF    
A Study on the Mechanical Properties of MAG Weld on Ferritic Stainless Steel Sheets
Gyeong-cheol Lee, Jae-seong Kim, Hyun-jae Kim, Kyoung-ho Lim, Bo-Young Lee
J Weld Join. 2009;27(2):27-31.   Published online May 18, 2009
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2026 by The Korean Welding and Joining Society.

Developed in M2PI