Effect of Welding Heat Input on the Simulated Heat-Affected-Zone Toughness for Yield Strength 390MPa Class TMCP Steel Plate
Ho-Seop Sim, Ki-Hyuk Kim, Joon-Ho Sung et al.
J Weld Join. 2024;42(3):292-297.   Published online June 30, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032340
Influence of Oxide Inclusions on the Creep Properties of Electron Beam Welds in Ti-added Reduced Activation Ferritic/Martensitic Steel
Jae-Yeon Han, Yoon-Hwan Jo, Chiwon Kim, Chang-Hoon Lee, Joonoh Moon, Hyun-Uk Hong
J Weld Join. 2024;42(3):282-291.   Published online June 30, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032298
A Study on the Microstructure and Mechanical Properties of SA508 Gr.3 Cl.1 Steel Cladded by a Laser Beam using Alloy 82 and 308L Powders for Small Modular Reactor
In-Chul Jung, Insung Choi, Kwang-Hyun Lee et al.
J Weld Join. 2023;41(6):429-439.   Published online December 31, 2023
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Solidification Cracking Susceptibility of the Weld Metal of Additively Manufactured 316L Stainless Steel
So-Young Park, Yongjoon Kang, Dongjin Oh, Sangwoo Song, Hyun-Uk Hong
J Weld Join. 2021;39(1):45-50.   Published online February 1, 2021
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Technical Issues in Fusion Welding of Reduced Activation Ferritic/Martensitic Steels for Nuclear Fusion Reactors
Sun-Young Jun, So-Young Im, Joonoh Moon, Chang-Hoon Lee, Hyun-Uk Hong
J Weld Join. 2020;38(1):47-55.   Published online February 26, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031916
Microstructure and Mechanical Properties in the Welds of Reduced-Activation Ferritic/Martensitic Steels
Joonoh Moon, Jinjong Lee, Chang-Hoon Lee et al.
J Weld Join. 2018;36(1):18-24.   Published online February 21, 2018
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031798
Influence of Gas Metal Arc Welding Parameters on the Bead Properties in Automatic Cladding
Mathieu TERNER, Tsend-Ayush BAYARSAIKHAN, Hyun-Uk Hong, Je-Hyun Lee
J Weld Join. 2017;35(1):16-25.   Published online January 19, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
PWHT Cracking Susceptibility in the Weld Heat-Affected Zone of Reduced Activation Ferritic/Martensitic Steels
Jinjong Lee, Joonoh Moon, Chang-Hoon Lee et al.
J Weld Join. 2016;34(6):47-54.   Published online December 29, 2016
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Microstructure and Creep Fracture Characteristics of Dissimilar SMA Welds between Inconel 740H Ni-Based Superalloy and TP316H Austenitic Stainless Steel
Kyeong-Yong Shin, Ji-Won Lee, Jung-Min Han, Kyong-Woon Lee, Byeong-Ook Kong, Hyun-Uk Hong
J Weld Join. 2016;34(5):33-40.   Published online October 30, 2016
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
A Study on the Improvement of Numerical Thermal Analysis for Steel Welds
Youn-Hee Kang, Choong-Myeong Kim, Hyun-Uk Hong, Jong-Bong Lee
J Weld Join. 2007;25(5):36-44.   Published online December 3, 2007
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2026 by The Korean Welding and Joining Society.

Developed in M2PI