Microstructural Characteristics of 800 ㎫ Grade High Strength Steel Weld Metals
Jaehee Lee, Sanghoon Kim, Byunghyun Yoon, Hwantae Kim, Sangcheol Kil, Changhee Lee
J Weld Join. 2011;29(1):65-73.   Published online March 4, 2011
PDFPDF    
Correlation Between M-A Constituents and Tensile Properties in the Intercritical Coarse Grained HAZ of an Ultra Low Carbon Steel
Yoonki Lee, Joonoh Moon, Sanghoon Kim, Changhee Lee
J Weld Join. 2010;28(3):99-103.   Published online August 2, 2010
PDFPDF    
Prediction Model for the Microstructure and Properties in Weld Heat Affected Zone : Ⅳ. Critical Particle Size for the Particle Coarsening Kinetics in Weld HAZ of Ti Added Low Alloyed Steel
Joonoh Moon, Sanghoon Kim, Hongchul Jeong, Jongbong Lee, Changhee Lee
J Weld Join. 2007;25(2):62-69.   Published online May 17, 2007
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI