2032480
Development of a Laser Processing System for Fuel Cell Bipolar Plates in Eco-Friendly Propulsion Applications and Evaluation of Cutting Performance
Su-Jin Lee, Ryoon-Han Kim, Danbi Song, Kwang-Deok Choi, Goo Cheol Kwon
J Weld Join. 2026;44(4):358-367.   Published online August 31, 2026
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032374
Laser Cutting Characteristics Using High-speed Camera of 75-㎛ Thick Stainless Steel Foil in Lightweight Fuel Cell Applications
Jung-Lo Yoon, Su-Jin Lee, Ryoon-Han Kim, Kwang-Deok Choi, NamHyun Kang, Danbi Song
J Weld Join. 2024;42(6):635-646.   Published online December 31, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Basic Study of Laser Direct Joining for CFRTP and Metals using High Power Diode Laser
Su-Jin Lee, Jong-Do Kim, Jeong SUH
J Weld Join. 2019;37(6):572-578.   Published online December 4, 2019
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031864
Research Trend of Laser Welding and Weldability of High Speed Dissimilar Laser Lap Welding for Titanium
Su-Jin Lee, Eunjoon Chun, Jeong SUH
J Weld Join. 2017;35(4):16-22.   Published online August 14, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031802
Influence of Metallic Sodium on Repair Weldability for Type 316FR Stainless Steel
Eun-Joon Chun, Su-Jin Lee, Jeong Suh, Ju-Seung Lee, Namhyun Kang, Kazuyoshi Saida
J Weld Join. 2017;35(1):79-88.   Published online February 15, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Solidification Cracking Behavior in Austenitic Stainless Steel Laser Welds (Part 1) - Evaluation of Solidification Cracking Susceptibility by Laser Beam Welding Varestraint Test -
Eun-Joon Chun, Su-Jin Lee, Jeong Suh, Namhyun Kang, Kazuyoshi Saida
J Weld Join. 2016;34(5):54-60.   Published online October 30, 2016
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031655
A Study on the Characteristic of Weld Joint and Tensile Fracture of SUS304 and Cu High-Speed Dissimilar Lap Welds by Single Mode Fiber Laser
Su-Jin Lee, Jong-Do Kim, Seiji Katayama
J Weld Join. 2014;32(6):592-599.   Published online December 31, 2014
PDFPDF    
Mechanical Properties of Cu and Ni Dissimilar Welds by High Welding Speed Using Single-Mode Fiber Laser
Su-Jin Lee, Jong-Do Kim
J Weld Join. 2014;32(3):295-302.   Published online June 30, 2014
PDFPDF    
2031537
Weldability of SUS304 and Ti Dissimilar Welds with Various Welding Speed using Single Mode Fiber Laser
Su-Jin Lee, Seiji Katayama, Jong-Do Kim
J Weld Join. 2013;31(5):64-70.   Published online November 5, 2013
PDFPDF    
A Study on Laser Assisted Machining for Silicon Nitride Ceramics (Ⅳ) - Mechanism and Application of LAM for Silicon Nitride Ceramics
Jong-Do Kim, Su-Jin Lee, Seo-Jeong Park, Jae-Hoon Lee
J Weld Join. 2010;28(6):40-44.   Published online January 10, 2011
PDFPDF    
A Study on Laser Assisted Machining for Silicon Nitride Ceramics (Ⅲ) - Variation of the Main Cutting Force and Life of Cutting Tool by LAM of SSN and HIPSN
Jong-Do Kim, Su-Jin Lee, Tae-Young Kang, Jeong Suh, Jae-Hoon Lee
J Weld Join. 2010;28(6):35-39.   Published online January 10, 2011
PDFPDF    
A Study on Laser Assisted Machining for Silicon Nitride Ceramics (Ⅱ) - Surface Characteristics of LAM Machined SSN and HIPSN
Jong-Do Kim, Su-Jin Lee, Tae-Young Kang, Jeong Suh, Jae-Hoon Lee
J Weld Join. 2010;28(5):80-85.   Published online November 5, 2010
PDFPDF    
A Study on Laser Assisted Machining for Silicon Nitride Ceramics (Ⅰ) - Preheating Characteristics and Oxidation Behaviors of Silicon Nitride Ceramics with Machining Parameters
Jong-Do Kim, Su-Jin Lee, Jeong Suh, Jae-Hoon Lee
J Weld Join. 2010;28(4):61-66.   Published online September 8, 2010
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2026 by The Korean Welding and Joining Society.

Developed in M2PI