Research Papers
2032080
A Study on Joint Properties of Sn-Cu-(X)Al-(Y)Si/Cu Solder by Multiple Reflow
Dong-Yurl Yu, Jun-Hyuk Son, Yong-Ho Ko, Chang-Woo Lee, Dongjin Byun, Junghwan Bang
J Weld Join. 2020;38(2):131-137.   Published online April 28, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032081
Laser-Assisted Bonding (LAB), Its Bonding Materials, and Their Applications
Kwang-Seong Choi, Jiho Joo, Ki-seok Jang et al.
J Weld Join. 2020;38(2):138-144.   Published online April 29, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032078
Effect of Underfill and Cornerfill on the 3-Point Bending Reliability of BGA Package Under Thermal Shock Test
Kyung-Yeol Kim, Haksan Jeong, Sang-Woo Kim, Jae-Oh Bang, Seung-Boo Jung
J Weld Join. 2020;38(2):145-151.   Published online April 22, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Influence of Carbon Nanotube Concentration on the Interconnection Properties of Solderable Isotropic and Anisotropic Conductive Adhesive
Byung-Seung Yim, Hee Jun Youn, Jeong Il Lee, Jong-Min Kim
J Weld Join. 2020;38(2):152-157.   Published online April 23, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Review Paper
Strategies to Reduce Transient Liquid Phase Bonding Time for the Die Attach of Power Semiconductors
Sunghyun Sohn, Daewon Kim, Hongpyo Kim, Namhyun Kang
J Weld Join. 2020;38(2):158-165.   Published online April 29, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Research Papers
Microstructure and Phase Analysis of Pure Ti and Ti-6Al-4V GTAW Cladding Material
Byung Hak Choe, Sang-Woo Lee, Tae-Woon Lim, Chung-In kim, Jae-Hwi Kim
J Weld Join. 2020;38(2):166-172.   Published online April 10, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
A Study on the Selection of Arc Sensing Signal for Seam Tracking in Pulsed GMAW
Bo Wook Seo, Young Cheol Jeong, Young Tae Cho
J Weld Join. 2020;38(2):173-179.   Published online April 8, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
The Effect of EP/EN Cycle Ratio on the Deposition Characteristics of Al 5183 Aluminum Alloys Fabricated by Variable Polarity WAAM
Henry Hwang, Tae-Hyun Lee, Cheolhee Kim, Soong Keun Hyun, Minjung Kang
J Weld Join. 2020;38(2):180-186.   Published online March 13, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Numerical Model for Powder Consumption, HAZ Width and Toughness in Tandem Submerged Arc Welding
M. H. Kakaei-Lafdani, M. Valehi
J Weld Join. 2020;38(2):187-196.   Published online April 1, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Effect of Laser Power Feedback Control on Mechanical Properties of Stainless Steel Part Built by Direct Energy Deposition
ChiYen Kim, JiSung Kim, Ho Lee et al.
J Weld Join. 2020;38(2):197-202.   Published online April 3, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
The Effect of Pre-Welding on Nugget Growth Behavior and Weldability for the Resistance Spot Welding of A6014 - T4 Alloy
Hyun-Uk Jun, Jae-Hun Kim, Joo-Yong Cheon, Young-Gon Kim, Yang-Do Kim, Changwook Ji
J Weld Join. 2020;38(2):203-210.   Published online March 11, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI