A Study on Development of the Optimization Algorithms to Find the Seam Tracking
Byeong-Ju Jin, Jong-Pyo Lee, Min-Ho Park, Do-Hyeong Kim, Qian-Qian Wu, Il-Soo Kim, Joon-Sik Son
J Weld Join. 2016;34(2):59-66. Published online 2016 Apr 30 DOI: https://doi.org/10.5781/JWJ.2016.34.2.59
|
Citations to this article as recorded by
Recent Research Trend of Arc Welding Quality Monitoring Technology in Korea
Young-Min Kim, Jason Cheon
Journal of Welding and Joining.2023; 41(2): 81. CrossRef Features for image processing of OCT images for seam tracking applications in laser welding
Thomas Will, Eric Eschner, Michael Schmidt
Journal of Laser Applications.2022;[Epub] CrossRef Study of Extraction Algorithm for Image Processing in Vertical GMA Welding
Chang-Gon Kim, Min-Ho Park, Joon-Sik Son, Tae-Jong Yun, Ill-Soo Kim
Journal of the Korean Society of Manufacturing Tec.2018; 27(4): 363. CrossRef
|