Effects of Fluoride in the Flux on Hydrogen Content in Weld Metal and Operating Behavior in FCAW-S
Woong Kil, Myeong-jun Shin, Kook-soo Bang
J Weld Join. 2017;35(5):65-70. Published online 2017 Sep 13 DOI: https://doi.org/10.5781/JWJ.2017.35.5.9
|
Citations to this article as recorded by
Flux Filling Rate Effect on Weld Bead Deposition of Recycled Titanium Chip Tubular Wire
Andrés M. Moreno-Uribe, José Gedael Fagundes, Izabel L. Criscuolo, Thomas Hassel, A. Q. Bracarense
International Journal of Precision Engineering and.2024;[Epub] CrossRef Effect of Flux Ratio on Droplet Transfer Behavior in Metal-Cored Arc Welding
Ngoc Quang Trinh, Shinichi Tashiro, Tetsuo Suga, Tomonori Kakizaki, Kei Yamazaki, Tomokazu Morimoto, Hiroyuki Shimizu, Ackadech Lersvanichkool, Hanh Van Bui, Manabu Tanaka
Metals.2022; 12(7): 1069. CrossRef Metal Transfer Behavior of Metal-Cored Arc Welding in Pure Argon Shielding Gas
Ngoc Quang Trinh, Shinichi Tashiro, Tetsuo Suga, Tomonori Kakizaki, Kei Yamazaki, Ackadech Lersvanichkool, Hanh Van Bui, Manabu Tanaka
Metals.2022; 12(10): 1577. CrossRef The Effect of Electrochemical Composite Coatings with LaF3-LaB6 Particles in Nickel–Copper Matrix on the Metallurgical Processes in Arc Welding of Low Alloy Ferrite-Pearlite Steels
Sergey G. Parshin, Victor A. Karkhin, Peter Mayr, Alexey S. Maystro
Materials.2021; 14(6): 1509. CrossRef Effects of alkaline elements on the metal transfer behavior in metal cored arc welding
Ngoc Quang Trinh, Shinichi Tashiro, Keigo Tanaka, Tetsuo Suga, Tomonori Kakizaki, Kei Yamazaki, Tomozaku Morimoto, Hiroyuki Shimizu, Ackadech Lersvanichkool, Anthony B. Murphy, Hanh Van Bui, Manabu Tanaka
Journal of Manufacturing Processes.2021; 68: 1448. CrossRef Effects of PTFE on operational characteristics and diffusible H and O contents of weld metal in underwater wet welding
Erriston Campos Amaral, Andrés M. Moreno-Uribe, Alexandre Queiroz Bracarense
Journal of Manufacturing Processes.2021; 61: 270. CrossRef Adição de TiO2, CaCO3 e CaF2 Como Componentes do Fluxo de Arames Tubulares para a Formação de TiC
José Gedael Fagundes Júnior, Alphonsus Henrique Clemente Cardoso, Alexandre Queiroz Bracarense
Soldagem & Inspeção.2020;[Epub] CrossRef Comparison of underwater wet welding performed with silicate and polymer agglomerated electrodes
Pedro Henrique Ribeiro Menezes, Ezequiel Caires Pereira Pessoa, Alexandre Queiroz Bracarense
Journal of Materials Processing Technology.2019; 266: 63. CrossRef Microstructure and mechanical properties of FCTIG-welded DH36 steel with rutile-type and basic-type flux cored wires
Lijun Yang, Yaowei Wang, Tao Sun, Yiming Huang, Yonglei Zhai, Tianxi He
Journal of Materials Processing Technology.2019; : 116363. CrossRef Efeitos da Espessura da Fita Metálica no Metal de Solda Utilizando Cavacos de Titânio Como Componentes do Fluxo em Arames Tubulares para a Formação de TiC
José Gedael Fagundes Júnior, Alexandre Queiroz Bracarense
Soldagem & Inspeção.2019;[Epub] CrossRef
|