Study on the Fracture Toughness of FCA Weldment with the Yield Strength 420MPa Grade High Strength Steels for Offshore Structures Depending on the Welding Position
In-Chan Kim, Sang-Hoon Jeong, Han-Geul Choi, Myung-Hyun Kim
J Weld Join. 2018;36(2):67-73.   Published online 2018 Apr 2     DOI: https://doi.org/10.5781/JWJ.2018.36.2.10
Citations to this article as recorded by Crossref logo
Role of bainitic microstructures with M-A constituent on the toughness of an HSLA steel for seismic resistant structural applications
Dileep Chandran Ramachandran, Joonoh Moon, Chang-Hoon Lee, Sung-Dae Kim, Jun-Ho Chung, Elliot Biro, Yeong-Do Park
Materials Science and Engineering: A.2021; 801: 140390.     CrossRef