![]() |
Vaporization Modeling and Experimental Verification During Laser Beam Welding for 24Mn Steel
Myeonghwan Choi, Daewon Cho, Namhyun Kang
J Weld Join. 2022;40(6):457-463. Published online 2022 Dec 30 DOI: https://doi.org/10.5781/JWJ.2022.40.6.1
|
Citations to this article as recorded by
Fatigue performance of hybrid laser arc welded joints with high manganese steel
Ji-Hoon Kim, Won-Chan Jeong, Insung Choi, Kwang-Hyeon Lee, Myung-Hyun Kim
International Journal of Naval Architecture and Oc.2025; 17: 100660. CrossRef Severe Mn vaporization for partial-penetrated laser keyhole welds of high-manganese cryogenic steel
Myeonghwan Choi, Dae-Won Cho, Kwang-Hyeon Lee, Seonghoon Yoo, Sangyong Nam, Namhyun Kang
International Journal of Heat and Mass Transfer.2024; 227: 125567. CrossRef A Study on Bead on Plate (BOP) Test for Laser Welding Application of Stainless Steel to Liquified Hydrogen Tank (PART I: STS 304)
Eul-Yong Ha, Chang-Min Pyo, Young-Hyun Kim, Jin-Seok Woo, Sun-Pil Kim, Myung-Su Yi, Sung-Wook Kang, Chang-Wook Ji, Jae-Woong Kim
Journal of Welding and Joining.2023; 41(6): 500. CrossRef Study on the Comparison of Electron Beam Welding and Hybrid Laser-Arc Welding of Thick High-Manganese Steel Plate for Cryogenic Applications
Insung Choi, Heon min Seo, In-Chul Jung, Kwang-Hyeon Lee, Jeong Suh
Journal of Welding and Joining.2023; 41(6): 528. CrossRef
|