Effects of Shielding Gases on the Weldability of Laser Welded Austenitic Stainless Steel
Yeonho Kwak, Seung Hwan Lee, Minjung Kang
J Weld Join. 2022;40(6):525-532.   Published online 2022 Dec 30     DOI: https://doi.org/10.5781/JWJ.2022.40.6.8
Citations to this article as recorded by Crossref logo
Mechanisms of Reverted Austenite and Grain Refinement via Neutron Diffraction for Enhancing Mechanical Properties of 304 Stainless Steel
Donghun Lee, Baek-Seok Seong, Byungrok Moon, Bong Cheon Park, Changhoon Lee, Sung-Dae Kim, Namhyun Kang
Metals and Materials International.2025;[Epub]     CrossRef
Effect of δ–ferrite and strain-induced martensite on hydrogen embrittlement of STS 308 L and STS 316 L all-weld metals
Donghyeon Choi, Jimin Nam, Byungrok Moon, Sourav Kr. Saha, Jaeseok Yoo, Jong Min Park, Kwang Hee Yun, Namhyun Kang
Corrosion Science.2024; 231: 111977.     CrossRef
Study on Columnar Grain Growth Mechanism of SUS439L Arc Welding
Jongho Jeon, Sangmin Lee, Woohyun Tak, Yoonsoo Lee, Injong Jin, Chaehun Han, Seungmin Baek, Inhwan Koo, Sungchae Cho, Jungho Cho
Journal of Welding and Joining.2024; 42(6): 595.     CrossRef
Weld Quality Analysis of High-Hardness Armored Steel in Pulsed Gas Metal Arc Welding
Hwi Jun Son, Young Cheol Jeong, Bo Wook Seo, Sung-Tae Hong, Yu-Chan Kim, Young Tae Cho
Metals.2023; 13(2): 303.     CrossRef