A Study on the Change of Wire Feeding Speed in GTA Welding (Ⅰ) - Changes in the Modes of Metal Transfer -
Daekyu Park, Jehyoung Cho, Youngwhan Park
J Weld Join. 2023;41(3):202-206.   Published online 2023 Jun 30     DOI: https://doi.org/10.5781/JWJ.2023.41.3.9
Citations to this article as recorded by Crossref logo
A Study on the Change of Wire Feeding Speed in GTA Welding (Ⅱ) - Development of Weld Bead Shape Prediction Model -
Daekyu Park, Changik Lee, Youngwhan Park
Journal of Welding and Joining.2023; 41(3): 207.     CrossRef