Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Effect of Groove Conditions on the Mechanical Properties of Welds Produced by the Combined Welding Process of Flux Cored Arc and Electro Gas in EH36 TMCP Steel Plate for Hull Structures
Kihyuk Kim, Kiwon Kim, Hoseop Sim, Kangho Bae, Hyunuk Hong, Byunggyu Park
JWJ. 2015;33(5):35-40.   Published online 2015 October 30    DOI: https://doi.org/10.5781/JWJ.2015.33.5.35

Excel Download

Flux Cored Wire Material Gas Shielded Arc Welding Thick Steel Plate Welded Crack Analysis
Advanced Materials Research. 2013;710:76-79   Crossref logo
Link1

Hardfacing of 3.5% Chromium Cast Steel by Flux Cored Wire Arc Welding Process
Key Engineering Materials. 2017;751:73-78   Crossref logo
Link1

Microstructure Transformation, Precipitation and Mechanical Properties of Nb Micro-Alloyed Shipbuilding Steel Plate EH36 Subjected TMCP
Key Engineering Materials. 2003;233-236:643-648   Crossref logo
Link1

The comparison of gas tungsten arc welding and flux cored arc welding effects on dual phase steel
Materials Research Express. 2020;7(3):036523   Crossref logo
Link1 Link2 Link3 Link4 Link5 Link6 Link7 Link8

Effect of Storage Conditions of Rutile Flux Cored Welding Wires on Properties of Welds
Advances in Materials Science. 2019;19(4):46-56   Crossref logo
Link1 Link2

Groove configurations of a flux-cored arc welding process used in critical structures of precision mechanical presses—mechanical and metallurgical studies
The International Journal of Advanced Manufacturing Technology. 2015;78(9-12):1905-1916   Crossref logo
Link1 Link2 Link3

Flux Cored Arc Welding
Welding Handbook. 1971;203-236   Crossref logo
Link1

Flux cored arc welding
Mig Welding Guide. 2006;80-89   Crossref logo
Link1 Link2 Link3

Effect of flux cored arc welding process parameters on bead geometry in super duplex stainless steel claddings
Measurement. 2015;62:127-136   Crossref logo
Link1 Link2

Effect of flux cored arc welding process parameters on duplex stainless steel clad quality
Journal of Materials Processing Technology. 2006;176(1-3):230-239   Crossref logo