Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW
Jin-Hyeong Park, Sung-Hwan Kim, Roh-Won Kim, Hyeong-Soon Moon, Myung-Hyun Kim
J Weld Join. 2019;37(4):333-338.   Published online 2019 July 22    DOI: https://doi.org/10.5781/JWJ.2019.37.4.7

Excel Download

A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW
Journal of Welding and Joining. 2019;37(6):605-605   Crossref logo
Link1 Link2 Link3

A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW
Journal of Welding and Joining. 2019;37(4):333-338   Crossref logo
Link1 Link2 Link3

Prediction of Welding Parameters and Weld Bead Geometry for GMAW Process in Overhead T-Fillet Welding Position (4F)
Advanced Materials Research. 2013;686:320-324   Crossref logo
Link1

A Brief Study of Unconventional Variants of GMAW Welding: Parameters, Weld Bead, and Microstructures
Engineering Principles - Welding and Residual Stresses. 2022;   Crossref logo
Link1

Influence of Heat Input and Welding Position on Geometrical Properties of GMAW Fillet Welds of Unalloyed Steel
TEM Journal. 2020;496-500   Crossref logo
Link1

Assessment of Weld Bead Performance for Pulsed Gas Metal Arc Welding (P-GMAW) Using Acoustic Emission (AE) and Machine Vision (MV) Signals Through NDT Methods for SS 304 Material
Volume 2A: Advanced Manufacturing. 2020;   Crossref logo
Link1 Link2

The Effect of EN Pulsing Ratio and Repetition Frequency on the Bead Appearance and Microstructure Evolution in Aluminum Welding using Variable Polarity GMAW
Journal of Welding and Joining. 2021;39(2):174-181   Crossref logo
Link1 Link2 Link3

Numerical Analysis of Forming Mechanism of Hump Bead in High Speed GMAW
Welding in the World. 2010;54(9-10):R286-R291   Crossref logo
Link1 Link2 Link3

Bead Geometry Prediction in Pulsed GMAW Welding: A Comparative Study on the Performance of Artificial Neural Network and Regression Models
Soldagem & Inspeção. 2022;27:   Crossref logo
Link1

A Study for TIG Welding Optimization on Bead Shape of A6061 Alloy Sheet using DOE
Journal of Welding and Joining. 2018;36(3):31-37   Crossref logo
Link1 Link2 Link3

This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014.