CrossRef Text and Data Mining
Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Influence of Carbon Nanotube Concentration on the Interconnection Properties of Solderable Isotropic and Anisotropic Conductive Adhesive
Byung-Seung Yim, Hee Jun Youn, Jeong Il Lee, Jong-Min Kim
JWJ. 2020;38(2):152-157.   Published online 2020 April 23    DOI: https://doi.org/10.5781/JWJ.2020.38.2.4

Excel Download

Influence of multi-walled carbon nanotube (MWNT) concentration on the interconnection properties of solderable anisotropic conductive adhesives (SACAs)
Journal of Materials Science: Materials in Electronics. 2015;26(7):4969-4980   Crossref logo
Link1 Link2 Link3

Thermo-mechanical reliability of a multi-walled carbon nanotube-incorporated solderable isotropic conductive adhesive
Microelectronics Reliability. 2016;57:93-100   Crossref logo
Link1 Link2

Influence of multi-walled carbon nanotube (MWCNT) concentration on the thermo-mechanical reliability properties of solderable anisotropic conductive adhesives (SACAs)
Microelectronics Reliability. 2018;91:201-212   Crossref logo
Link1 Link2

Reliability Properties of Carbon Nanotube-filled Solderable Anisotropic Conductive Adhesives
Journal of Welding and Joining. 2017;35(3):15-20   Crossref logo
Link1 Link2 Link3

Effect of dispersion condition of multi-walled carbon nanotube (MWNT) on bonding properties of solderable isotropic conductive adhesives (ICAs)
Journal of Materials Science: Materials in Electronics. 2014;25(12):5208-5217   Crossref logo
Link1 Link2 Link3

Flip Chip Assembly Using Carbon Nanotube Bumps and Anisotropic Conductive Adhesive Film
ECS Transactions. 2019;27(1):825-830   Crossref logo
Link1 Link2 Link3 Link4 Link5

Effect of multi-walled carbon nanotube (MWCNT) concentration on thermomechanical reliability of MWCNT-reinforced solderable isotropic polymer nanocomposites
Journal of Materials Science: Materials in Electronics. 2016;27(9):9159-9171   Crossref logo
Link1 Link2 Link3

Influence of functionalized graphene on the electrical, mechanical, and thermal properties of solderable isotropic conductive adhesives
Journal of Materials Science: Materials in Electronics. 2016;27(5):4516-4525   Crossref logo
Link1 Link2 Link3

Coalescence Characteristics of Fusible Particles in Solderable Isotropic Conductive Adhesives (ICAs)
Materials Science Forum. 2008;580-582:213-216   Crossref logo
Link1

Development and Application of Low-Temperature Curable Isotropic Conductive Adhesive Toward to Fabrication in IoT Generation
Applied Adhesive Bonding in Science and Technology. 2018;   Crossref logo
Link1

This metadata service is kindly provided by CrossRef from May 29, 2014. Journal of Welding and Joining has participated in CrossRef Text and Data Mining service since October 29, 2014.