CrossRef Text and Data Mining |
Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining. |
Effects of Mo and Nb on Microstructure and Charpy Impact Properties of CGHAZ in HSLA Steels |
Min Gu Kim, Sung Kyu Cho, Sang Yong Shin |
J Weld Join. 2022;40(1):22-32. Published online 2022 February 22 DOI: https://doi.org/10.5781/JWJ.2022.40.1.3 |
Effects of Mo and Nb on Microstructure and Charpy Impact Properties of CGHAZ in HSLA Steels Effects of Nb or (Nb + Mo) alloying on Charpy impact, bending, and delayed fracture properties in 1.9-GPa-grade press hardening steels Microstructures and Continuous Cooling Transformation of CGHAZ in E36 Class V-N-Ti, V-Ti and Nb-Ti Shipbuilding Steels Effect of Mo Addition on the Precipitation Behavior of Carbide in Nb-Bearing HSLA Steel Effect of Niobium Content on the Microstructure and Mechanical Properties of Simulated Coarse-Grained Heat-Affected Zone (CGHAZ) of High-Strength Low-Alloy (HSLA) Steels The Influence of Mo, Cr and B Alloying on Phase Transformation and Mechanical Properties in Nb Added High Strength Dual Phase Steels Microstructure and Mechanical Properties of Nb Microalloyed Q370qE-HPS Bridge Steel Produced by TMCP Quantifying the Effect of Nb and Mo on Transformation Products Using Advanced EBSD Analysis Effects of Microstructure on Tensile, Charpy Impact, and Crack Tip Opening Displacement Properties of Two API X80 Pipeline Steels Effect of Heat-Input on Microstructure and Toughness of CGHAZ in a High-Nb-Content Microalloyed HSLA Steel |
This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014. |