Result of CrossRef Text and Data Mining Search is the related articles with entitled article. If you click link1 or link2 you will be able to reach the full text site of selected articles; however, some links do not show the full text immediately at now. If you click CrossRef Text and Data Mining Download icon, you will be able to get whole list of articles from literature included in CrossRef Text and Data Mining.
Residual Stress and Deformation Characteristics by FSW and SAW of Wear Resistant Steel
Jeongung Park, Gyubaek An, Dusan Kim
J Weld Join. 2022;40(2):133-140.   Published online 2022 April 21    DOI: https://doi.org/10.5781/JWJ.2022.40.2.4

Excel Download

Residual Stress and Deformation Characteristics by FSW and SAW of Wear Resistant Steel
Journal of Welding and Joining. 2022;40(2):133-140   Crossref logo
Link1 Link2 Link3

Characterization and residual stress analysis of wear resistant Mo thermal spray-coated steel gear wheels
Surface and Coatings Technology. 2006;200(14-15):4266-4276   Crossref logo
Link1 Link2

A mechanical explanation for the influence of residual stress on the wear resistance of borided steel
Wear. 1990;137(2):151-159   Crossref logo
Link1 Link2

The residual stress, texture and surface changes in steel induced by cavitation
Wear. 1991;150(1-2):11-20   Crossref logo
Link1 Link2

Effect of cooling rate on microstructure, hardness, and residual stress of 0.28C–0.22Ti wear-resistant steel
Journal of Iron and Steel Research International. 2019;26(8):866-874   Crossref logo
Link1 Link2 Link3

Study on Wear-Resistant Steel Quenching Deformation
Advanced Materials Research. 2010;145:347-352   Crossref logo
Link1

Influence of Heat Treatment on Residual Stress Formation in the Wear-Resistant Steel 60–Steel 15–Steel 60 Bimetal Material
Inorganic Materials: Applied Research. 2021;12(1):5-9   Crossref logo
Link1 Link2 Link3

A proposed diffusion-controlled wear mechanism of alloy steel friction stir welding (FSW) tools used on an aluminum alloy
Wear. 2014;318(1-2):130-134   Crossref logo
Link1 Link2

Deformation Control in Wear-Resistant Steel Quenching Process
Applied Mechanics and Materials. 2011;52-54:595-600   Crossref logo
Link1

Experimental investigation on deformation and wear of WC tool during friction stir welding (FSW) of stainless steel
The International Journal of Advanced Manufacturing Technology. 2014;73(1-4):479-486   Crossref logo
Link1 Link2 Link3

This metadata service is kindly provided by CrossRef from May 29, 2014. J Weld Join has participated in CrossRef Text and Data Mining service since October 29, 2014.