Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Design of Cylinder Horn for Ultrasonic Welding

Journal of KWJS 2009;27(4):60-66.
Published online September 14, 2009.
초음파 용접용 실린더 혼의 설계
, ,
 
Design of Cylinder Horn for Ultrasonic Welding
Sun-Rak Kim, JaeHak Lee, ChoongD. Yoo
Abstract
  The cylinder horn is designed to increase uniformity of the displacement on the output face through simulation and experiments for the simple cylinder, spool and step horns. The modal analysis is conducted numerically to calculate the vibration mode and stress distribution of the cylinder horn, and the design of experiment (DOE) technique is employed to determine the optimum configuration of the spool horn. Displacement of the cylinder horn was measured using the Laser Doppler Vibrometer (LDV), and experimental results show good agreements with the predicted results. It appears that uniformity higher than 95% can be achieved with the spool horn when the proper dimension of the groove is used.
Key Words: Ultrasonic welding, Horn design, Cylinder and Spool horn, Step horn


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI