ABSTRACT
  Pipe welding is used in various ranges such as civil engineering and ship building engineering. Until now, many technicians work for pipe welding manually under harmful, dangerous and difficult conditions. So it is necessary to install automation process. For automation pipe welding, relation between welding parameters & bead shape should be considered. Using this relation, bead shape could be expected from welding parameters. FCAW was used in this study. Instead of pipe workpiece, fillet joint plate is used, which were inclined 0,45,90,135,180 degree. By analyzing between welding parameters (current, welding speed, voltage) and bead shape parameters with non-linear multiple regression, bead shape parameters could be expected. Piecewise Cubic Hermite Interpolation was used to expect smooth curved bead shape with bead shape parameters. From these processes, bead shape could be expected from welding parameters.
Keywords: Bead shape;Welding parameter;Non linear regression;Taguchi-method;Piecewise cubic Hermite interpolation
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,322
View
0
Download
Related article
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI