Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Development of Knowledge-based Method to Automatically Derive the Deformation Estimation Formula due to Line Heating

Journal of KWJS 2010;28(1):92-99.
Published online March 10, 2010.
선상가열 변형예측식 자동 산출을 위한 지식기반 방법의 개발
 
Development of Knowledge-based Method to Automatically Derive the Deformation Estimation Formula due to Line Heating
Joo-Sung Lee
Abstract
  For the last couple of decades many studies have been carried out to find out solutions to improve the effectiveness and productivity of the plate forming process. The practical way for the automation of the plate forming process has not been, however, developed yet. Since the characteristics of heating machines may be different form each other, it is necessary to investigate the thermal deformation characteristics of the heating machine to be used in the automation system. And their characteristics may be updated as new information about thermal deformation by heating is accumulated. In this paper, data base system has been constructed based on the results of experiments and numerical analyses, which will be used in deriving the deformation estimation formula. The computer code which can automatically derive the deformation estimation formula has been also developed. This paper also illustrates how the formula is updated as experimental data are added. From the present findings, it can be said that the automatic deriving procedure may be important in the automated plate forming system since the heating line information to be generated must be directly influenced by the deformation estimation formula.
Key Words: Angular distortion, Automatic deriving system, DB system, Line heating, Thermo elastolastic analysis, Transverse shrinkage
TOOLS
METRICS Graph View
  • 1,536 View
  • 0 Download
Related articles


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI