Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Analytical Methodology Obtaining an Optimal Welding Sequence for Least Distortion of Welded Structure

J Weld Join > Volume 31(3); 2013 > Article
Journal of KWJS 2013;31(3):54-59.
DOI: https://doi.org/10.5781/KWJS.2013.31.3.54    Published online June 30, 2013.
Analytical Methodology Obtaining an Optimal Welding Sequence for Least Distortion of Welded Structure
Yunsok Ha
Correspondence:  Yunsok Ha,
Email: yunsok.ha@samsung.com
Abstract
Several methodologies analyzing welding distortions of large shell structures like ship blocks have been developed and utilized in shipyards for a long times ago. In general, one of objects of thermal distortion analysis is to find welding sequence making least-deformation without any suppliance, and it can be solved easily and rapidly by EP strain-boundary method. But after assembly construction, there are usually more than 10 weldments in each process, and the number of sequence will follow the Factorial calculation. In this research, a method has been suggested to decide the best welding sequence by minimum analysis. Using this method, welding deformation could be reduced just analyzing some cases as many as the number of weldments. Experiments and Analysis of all cases were also done, and their best results are good agreements with predictation by suggested methodology.
Key Words: Ship block, Wedling distortion, Shell element, FEM, Sequence


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI