Laser Stitch Welding Technology for the Fabrication of Automotive Parts
Sung-Min Joo1, Hee-Seon Bang2, Jun-Ui Han3, Kyoung-Hak Kim3, Byoung-Ho Ahn4
1Research Institute of Industrial Science & Technology, Plant R&D Division, Ulsan 683-420, Korea
2Department. of Naval Architecture & Ocean Engineering, Chosun University, Kwangju 501-759, Korea
3Graduate School of Naval Architecture & Ocean Engineering, Chosun University, Kwangju 501-759, Korea
4Gwang Il Machine, Kwangju 506-301, Korea
Correspondence: Hee-Seon Bang  Email: banghs@chosun.ac.kr
  Published online August 31, 2013
ABSTRACT
Nowadays, the weight lightening of automotive is required as conserving the environment has become a major worldwide issue. To solve this issue, various researches for the use of light materials(Alalloy, Mgalloy)and ultra high strength steel as substitutes of the current structural material have been carried out. Application of laser stitch welding to the assembly of automotive produces improvement in strength, lightening of body, higher fuel efficiency, lower production cost as well as reduction in assemble line due to its fast welding speed, superior accessible and weld quality. This process overcomes the shortcomings of the current resistance spot welding such as high electricity consumption, electrode replacement, and economical, technical limitation in design and production method of automotives.
Keywords: Laser stitch welding | Weight lightening | Weld quality | Automotives
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1
Crossref
1,600
View
6
Download
Related articles
High Efficient Welding Technology of the Car Bodies  2016 August;34(4)
High Speed TSV Filling Technology by using Molten Solder and Fabrication of Composite Solder as Filler Material  2012 June;30(3)
Laser Welding of Automotive Transmission Components  2011 December;29(6)
Development of Knowledge Sharing Platform for Welding Technology for the Automotive Industry  2011 October;29(5)
Laser Beam Welding Technology of Seal Tube for Radiation-Resistant LVDT Manufacturing  2011 October;29(5)
High Efficient Welding Technology of the Car Bodies  2016 August;34(4)
High Speed TSV Filling Technology by using Molten Solder and Fabrication of Composite Solder as Filler Material  2012 June;30(3)
Laser Welding of Automotive Transmission Components  2011 December;29(6)
Development of Knowledge Sharing Platform for Welding Technology for the Automotive Industry  2011 October;29(5)
Laser Beam Welding Technology of Seal Tube for Radiation-Resistant LVDT Manufacturing  2011 October;29(5)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI