Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Bonding Mechanism and Strength of Metals to Ceramics

J Weld Join > Volume 32(1); 2014 > Article
Journal of Welding and Joining 2014;32(1):40-46.
DOI: https://doi.org/10.5781/JWJ.2014.32.1.40    Published online February 27, 2014.
Bonding Mechanism and Strength of Metals to Ceramics
Se-Ho Kee*, Jae-Pil Jung*, Won-Joong Kim*
Correspondence:  Won-Joong Kim,
Email: wjkim@uos.ac.kr
Abstract
Bonding technology and bonding mechanism of metal to ceramic including brazing, diffusion bonding, friction welding and etc were reviewed in this study. Various factors should be considered from a bonding design step to acquire a good bonding joint because of a large difference between metal and ceramic in crystal lattice, coefficient of thermal expansion and various properties. In addition, metal and ceramic bonding technologies are constantly being developed according to precise components, multi-function and application to harsh environment. However, improvement of bonding properties and bonding reliability also should be accompanied. Bonding of ceramics, such as ZrO2, Ti3AlC2 and SiC, to metals like Ti-alloy, TiAl and steel were described in this paper.
Key Words: Active metal brazing, Ceramics, Bonding mechanism, Wettability, Residual stress


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI