Recent Study of Thermal Spray for Green Automotive Industry
Ho-Cheon Yoo*,†
*,†KISTI ReSEAT Program, Daejeon 305-806, Korea
Correspondence: Ho-Cheon Yoo  Email: yooho278@reseat.re.kr
  Published online June 30, 2014
ABSTRACT
Recent developing tendency of thermal spray for green automotive industry are studied by searching of NDSL, KIPRIS, ScienceDirect and so on. Spraying techniques such as plasma spray, microwave treatment, dry-ice blasting, HVOF thermal spray, cold spraying, aerosol deposition are introduced, further more spraying materials such as nano particles, intermetallic compound, TiAlN, TiC, Si-Al alloys are investigated.
Keywords: Thermal spray | Automotive | Plasma spray | Intermetallic compound | Cold spraying | HVOF
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
1,508
View
9
Download
Related articles
Recent Study of Technical Development for High Efficient Brazing  2016 April;34(2)
Recent Study of TiAl Brazing  2012 December;30(6)
Recent Study of Overlay Welding on Welding methods  2013 February;31(1)
Development of Knowledge Sharing Platform for Welding Technology for the Automotive Industry  2011 October;29(5)
Welding Technology of Magnesium Alloy for Automobile Industry  2004 June;22(3)
Recent Study of Technical Development for High Efficient Brazing  2016 April;34(2)
Recent Study of TiAl Brazing  2012 December;30(6)
Recent Study of Overlay Welding on Welding methods  2013 February;31(1)
Development of Knowledge Sharing Platform for Welding Technology for the Automotive Industry  2011 October;29(5)
Welding Technology of Magnesium Alloy for Automobile Industry  2004 June;22(3)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI