ABSTRACT
Nowadays, car manufacturers tried to improve automotive fuel efficiency, and applied many high strength steels such as AHSS or UHSS to car bodies. Therefore, the number of steel combinations for the resistance spot welding are dramatically increased and the need for weldability evaluation of these combinations are also required. In this study, we suggest the lobe curve using FEM simulations for DP780 steel with 1.0t, 1.4t. The lobe curves which could expressed weldablity and optimal welding condition were obtained according to 6 steel combinations. There were two combinations for same steel sheet which were DP780 1.0t, DP780 1.4t. Dissimilar steel sheet combination with different thickness was 1.0t and 1.4t of DP780. Different steel combinations were DP780 1.0t and SPRC440 1.0t, and DP780 1.0t and DP590 1.0t. Finally dissimilar combinations was and DP780 1.0t and DP590 1.4t. The trend of low boundary and high boundary variation of lobe curve were analyzed with a viewpoint of the contact resistance and the heat input.
Keywords: Resistance spot welding | Advanced high strength steel | Weld lobe curve | Nugget formation | Tensile shear strength
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1
Crossref
1,310
View
20
Download
Related articles
Predicting Failure Modes of Resistance Spot Welds from the Chemical Composition of Materials  2020 October;38(5)
Optimization of Welding Parameters in Resistance Spot Welding of 980 MPa Grade GA Steel Sheet using Multi-Response Surface Methodology  2018 August;36(4)
Evaluation on Resistance Spot Weldability and Nugget Formation of Surface Roughness Treated Steel Sheet  2008 October;26(5)
A Study of Dynamic Characteristic for Resistance Spot Welding Process Using Servo-gun System  2005 June;23(3)
A Study on Resistance Spot Welding of Dissimilar Sheet Metals ( Aluminum Alloy - Steel Sheets )   1997 August;15(4)
Predicting Failure Modes of Resistance Spot Welds from the Chemical Composition of Materials  2020 October;38(5)
Optimization of Welding Parameters in Resistance Spot Welding of 980 MPa Grade GA Steel Sheet using Multi-Response Surface Methodology  2018 August;36(4)
Evaluation on Resistance Spot Weldability and Nugget Formation of Surface Roughness Treated Steel Sheet  2008 October;26(5)
A Study of Dynamic Characteristic for Resistance Spot Welding Process Using Servo-gun System  2005 June;23(3)
A Study on Resistance Spot Welding of Dissimilar Sheet Metals ( Aluminum Alloy - Steel Sheets )   1997 August;15(4)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI