Published online October 30, 2015.
doi:https://doi.org/10.5781/JWJ.2015.33.5.35
Effect of Groove Conditions on the Mechanical Properties of Welds Produced by the Combined Welding Process of Flux Cored Arc and Electro Gas in EH36 TMCP Steel Plate for Hull Structures
Kihyuk Kim*, Kiwon Kim**, Hoseop Sim*, Kangho Bae*, Hyunuk Hong***, Byunggyu Park*
*Plate Research Team, Plate Business Division, Dongkuk Steel, Dangjin 343-823, Korea
**Dept. of Material Science Engineering, Pusan National Univ., Busan 609-735, Korea
***Dept. of Metallurgy and Materials Engineering, Changwon National Univ., Changwon 641-773, Korea
Correspondence: Byunggyu Park  Email: byunggyu.park@dongkuk.com
  Published online October 30, 2015
ABSTRACT
Characterization of microstructures and mechanical properties of 83mm thickness EH36-TM welds produced by the combined flux cored arc (FCA) and electro gas (EG) welding processes has been studied with the two different groove conditions, single-V (SV) and double-V (DV) bevels. The welding consumables used for FCA and EG welding processes were ASME/AWS A5.29 (E81T1-K2) and A5.26 (EG72T), respectively. Experimental results showed that all the mechanical properties of welds such as tensile property, CVN toughness and Vickers hardness met IACS requirements. The tensile strength of EG welded plates were reduced by approximately 4% (DV: 3.8%, SV: 4.2%) compared to the base metal. The hardness value of SV-beveled weld metal was slightly lower than that of DV-beveled one. There were no significant differences as per welding groove conditions except for the weld metal. In addition, at the fusion line, the toughness of SV condition was 20J lower and the weld metal was 40J lower than DV condition, respectively. On the basis of microstructural analysis, grain boundary ferrite (GBF) structures for SV condition were 2 times higher volume fraction than for DV condition and their packet sizes were coarsened to almost double. It was thus suggested that the GBF volume fractions and packet sizes in the weld metal of EH36-TM steel plates are the most important factors affecting the mechanical properties of the combined FCA and EG welded joint. Nevertheless, all the results of welds with both DV and SV conditions were found to be excellent.
Keywords: TMCP | Combined Welding | Groove Condition | Toughness | GBF
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
1,935
View
22
Download
Related article
Effects of Heat Inputs on the Mechanical Properties of FCA Weldment of YP 690MPa Grade Steels  2016 December;34(6)
Effects of Heat Inputs on the Mechanical Properties of FCA Weldment of YP 690MPa Grade Steels  2016 December;34(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI