Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 An Analytical Solution for Transient Temperature Distribution in Fillet Arc Welding Including the Effect of Molten Metal

Journal of KWJS 1995;13(3):116-124.
Published online September 25, 1995.
용착 금속을 고려한 필릿 용접에서 온도 분포 예측을 위한 해석적 모델
,
 
An Analytical Solution for Transient Temperature Distribution in Fillet Arc Welding Including the Effect of Molten Metal
정선국, 조형석