Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Hot Cracking in Austenitic Stainless Steel Welds

Journal of KWJS 1999;17(5):10-19.
Published online October 25, 1999.
특집 : 철강 및 비철합금의 고온균열 현상 ; 오스테나이트계 스테인리스강 용접부의 고온균열
,
 
Hot Cracking in Austenitic Stainless Steel Welds