Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-05.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Thermal Sprayed AlSiMg/TiC Composite Coatings : Fabrication of Powder and Characteristics of Coatings(Ⅰ)

Journal of KWJS 2000;18(5):98-104.
Published online October 25, 2000.
AlSiMg/TiC 복합 용사 피막 : 분말제조 및 피막 특성 (Ⅰ)
, ,
 
Thermal Sprayed AlSiMg/TiC Composite Coatings : Fabrication of Powder and Characteristics of Coatings(Ⅰ)
양병모, 변응선, 박경채