JWJ > Volume 19(1); 2001 > Article
Journal of KWJS 2001 February;19(1) :75-81.
Published online February 26, 2001.
Metallurgical Study of Microconstituents in Transient Liquid Phase Bonded Joints of Ni Base Superalloy
김대업
Correspondence:   Published online February 26, 2001
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
939
View
0
Download
Related articles
Transient Liquid Phase Bonding of Gamma Prime Precipitation Strengthened Ni Based Superalloy  2017 June;35(3)
Effect of Bonging Temperature and Heating Rate on Transient Liquid Phase Diffusion Bonding of Ni-Base Superalloy  2005 April;23(2)
Transient Liquid Phase Bonding of Directionally Solidified Ni Base Superalloy, GTD-111(III)  2003 June;21(3)
Transient Liquid Phase Bonding of Directionally Solidified Ni Base Superalloy, GTD-111(II)  2003 April;21(2)
Transient Liquid Phase Bonding of Directionally Solidified Ni Base Superalloy, GTD-111(I)  2003 April;21(2)
Transient Liquid Phase Bonding of Gamma Prime Precipitation Strengthened Ni Based Superalloy  2017 June;35(3)
Effect of Bonging Temperature and Heating Rate on Transient Liquid Phase Diffusion Bonding of Ni-Base Superalloy  2005 April;23(2)
Transient Liquid Phase Bonding of Directionally Solidified Ni Base Superalloy, GTD-111(III)  2003 June;21(3)
Transient Liquid Phase Bonding of Directionally Solidified Ni Base Superalloy, GTD-111(II)  2003 April;21(2)
Transient Liquid Phase Bonding of Directionally Solidified Ni Base Superalloy, GTD-111(I)  2003 April;21(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI