Analysis of Heat Flow and Deformation in Laser Welding of Small Gas Pressure Vessel
박상국, 김재웅, 김기철


Correspondence:   Published online February 26, 2001
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
934
View
0
Download
Related articles
Characteristic of Welding Rotational Deformation in Laser Welding of Thin Steel Sheet  2018 December;36(6)
3D Finite Element Analysis of Friction Stir Welding of Al6061 Plates  2011 August;29(4)
Development Trend of Steel and Welding Consumables for Pressure Vessel  2010 April;28(2)
Numerical Analysis of Heat Flow and Thermal Deformation in Transmission Joining of Polymers Using Nd:YAG Laser  2006 December;24(6)
The Analysis of Welding Deformation in Large Welded Structure by Using Local & Global Model  2004 December;22(6)
Characteristic of Welding Rotational Deformation in Laser Welding of Thin Steel Sheet  2018 December;36(6)
3D Finite Element Analysis of Friction Stir Welding of Al6061 Plates  2011 August;29(4)
Development Trend of Steel and Welding Consumables for Pressure Vessel  2010 April;28(2)
Numerical Analysis of Heat Flow and Thermal Deformation in Transmission Joining of Polymers Using Nd:YAG Laser  2006 December;24(6)
The Analysis of Welding Deformation in Large Welded Structure by Using Local & Global Model  2004 December;22(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI