Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Measurement of GMAW Bead Geometry Using Biprism Stereo Vision Sensor

Journal of KWJS 2001;19(2):63-70.
Published online April 25, 2001.
바이프리즘 스테레오 시각 센서를 이용한 GMA 용접 비드의 3차원 형상 측정
, ,
 
Measurement of GMAW Bead Geometry Using Biprism Stereo Vision Sensor
이지혜, 이두현, 유중돈