Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 The Influence of Chemical Compositions of Weld Metal and Welding Condisions on Hot Cracking by Hot Cracking Test

Journal of KWJS 2002;20(3):74-83.
Published online June 25, 2002.
Inconel 690 오버레이용접부의 고온균열 발생에 미치는 용접금속의 화학조성 및 용접조건의 영향
, , , , ,
 
The Influence of Chemical Compositions of Weld Metal and Welding Condisions on Hot Cracking by Hot Cracking Test
양병일, 지병하, 김정태, 박광식, 최해수, 박화순