Effects of Nitrogen on the Microstructure and Tonghness of HAZ in Ti-Containing Steel
김병철, 방국수

Correspondence:   Published online June 25, 2002
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,148
View
0
Download
Related articles
Correlation Between HAZ Microstructure and Low Temperature Impact Toughness of Bainitic Steel Plates  2021 June;39(3)
Effect of Microstructure on Low-Temperature Impact Toughness of Multi-Pass Weld Metal of 1 GPa Class High Strength Steel  2021 June;39(3)
Microstructure and Phase Analysis of Pure Ti and Ti-6Al-4V GTAW Cladding Material  2020 April;38(2)
The Effect of Heat Treatment on Microstructure and Mechanical Behaviors of Laser Direct Energy Deposited Ti-6Al-4V Plate  2018 October;36(5)
Effect of Tensile Properties and Microstructure on the Heat Input of Ni-Doped High Manganese Welding Wire  2018 February;36(1)
Correlation Between HAZ Microstructure and Low Temperature Impact Toughness of Bainitic Steel Plates  2021 June;39(3)
Effect of Microstructure on Low-Temperature Impact Toughness of Multi-Pass Weld Metal of 1 GPa Class High Strength Steel  2021 June;39(3)
Microstructure and Phase Analysis of Pure Ti and Ti-6Al-4V GTAW Cladding Material  2020 April;38(2)
The Effect of Heat Treatment on Microstructure and Mechanical Behaviors of Laser Direct Energy Deposited Ti-6Al-4V Plate  2018 October;36(5)
Effect of Tensile Properties and Microstructure on the Heat Input of Ni-Doped High Manganese Welding Wire  2018 February;36(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI