Comparison of Powder Feeding and Wire Feeding in Laser Cladding2013 August;31(4)
Monitoring Technology in Laser Welding2009 February;27(1)
Improvement of Gap Bridging Ability in CO₂ Laser-GMA Hybrid Welding2006 October;24(5)