Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Effect of He Mixing Ratio on the Characteristic of TIG Welding with High Current and High Speed

Journal of KWJS 2005;23(3):54-60.
Published online July 15, 2005.
[연구논문]대전류 고속 TIG 용접 특성에 미치는 He 혼합비의 영향
, ,
 
Effect of He Mixing Ratio on the Characteristic of TIG Welding with High Current and High Speed
Dong-Soo Oh, Yeong-Sik Kim, Sang-Myung Cho
Abstract
Tungsten Inert Gas(TIG) welding is today one of the most popular are welding process because of its high quality welds and low equipment costs. Even if welding productivity increases with welding speed and current, this strategy is limited by the appearance of defects such as undercut and humping bead due to the depressed molten metal. The purpose of this study investigates the effects of He mixing ratio on the characteristics with high current and speed in TIG welding. The conclusions obtained permit to explain the are start characteristics quantitatively and the maximum welding speed on stable bead formation with He mixing ratio for high current and speed TIG welding observed in experiments. Also through the relation of the maximum are pressure and surface depression depth at high current and speed TIG welding, it made clear the mechanism of unstable bead formation.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2024 by The Korean Welding and Joining Society.

Developed in M2PI