Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2025-06.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 100 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 101 Three Dimensional Analysis of Induction Heating Process using a Moving Coordinate

Journal of KWJS 2007;25(1):24-29.
Published online March 26, 2007.
이동좌표계를 이용한 3차원 유도가열공정 해석
, ,
 
Three Dimensional Analysis of Induction Heating Process using a Moving Coordinate
Jin-Oh Yun, Young-Soo Yang, Hee-Yun Shin
Abstract
  Finite element analysis for induction heating proces including magnetic and thermal situations is presented. Because magnetic and thermal material properties vary with the temperature, material properties depending on temperature are considered. As the inductor moves, the solution domains corresponding to the inductor change into those of the air and the solution domains corresponding to the air change into those of the inductor. For these reasons, modeling of induction heating proces is very dificult with a general purpose comercial programs. In this paper, three dimensional analysis of induction heating proces for moving inductor is analyzed using moving coordinate. The skin efect is confirmed inside the steel plate in the electro-magnetic analysis. The distribution of heat generation at the initial state is diferent from that at the quasi-stationary state. Therefore, material properties depending on temperature must be considered. The calculated results of finite element analysis agree well with the experimental temperature results. This aproach is suitable to solve magneto-thermal coupled problems.
Key Words: Induction heating, Moving coordinate, Finite element analysis


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2025 by The Korean Welding and Joining Society.

Developed in M2PI