Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Ways to Improve Reliability against Stress-Relief Cracking in Weld Metal

Journal of KWJS 2007;25(2):3-5.
Published online May 17, 2007.
용착금속부 재열균열에 대한 신뢰성 확보대책
,
 
Ways to Improve Reliability against Stress-Relief Cracking in Weld Metal
Hee-Jin Kim, Hoi-Soo Ryoo
TOOLS
METRICS Graph View
  • 1,449 View
  • 0 Download
Related articles

Analysis of Restraint Stress Acting on the Weldment 1997 February;15(1)